Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 67.6 MPa | 9800 psi | 1.3 mm/min; ASTM D790 |
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
PolyOne Edgetek® XT XT-500-CX02 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | Perpendicular |
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Luriblend® POM CO TL20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composit.. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Luriblend® POM CO TS20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Plastiblend® ABS 8004 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Plastiblend® ABS 8004 UV MB Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceTPCI# 6816121Information provided by TP Composites, Inc. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Plastiblend® ABS 8012 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Plastiblend® ABS 8014 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Luriblend® POM CO TL20 LE Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction, Low Extractables and CopolymerUL File Number: E.. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Plastiblend® ABS 8004 Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Techmer ES Plastiblend® ABS IM Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Chesterton ARC 897 Fine Grade Sliding Wear Compound Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t.. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Ensinger Tecamid® ST Nylon (PA) Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Ensinger Tecapeek® XP-91BST Compression Molded PEEK ST Compound, 30% Fiberglass, Black Pigmented Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D-790 |
Axiall HF-6597 Rigid PVC, Molding Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information provide.. |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-15FG-1734 15% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 67.6 MPa | 9800 psi | ASTM D790 |
Asahi Kasei Thermylene® P1-10FG-8100 10% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |