Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 58.6 MPa | 8500 psi | ASTM D790 |
PolyOne Maxxam™ PPH-10G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Polymer Resources ABS-FR1 ABS, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Total 620 Polystyrene
(discontinued **) Polystyrene 620 is an impact polystyrene designed for high gloss cap layers. The polymer has been specifically designed for co extrusion processing to produce a ductile sheet with an extremely high .. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | ASTM D790 |
PolyOne Edgetek® SY-15GB/000 Polystyrene (PS), Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | ASTM D790 |
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | ASTM D790-95 |
Multibase Multi-ABS 3259 Plating Grade Data provided by Multibase. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 511 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio.. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | |
SGL Carbon Group EK 2230 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | |
SGL Carbon Group EK 24 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | |
SGL Carbon Group EK 3235 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | |
SGL Carbon Group V 1626 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Techmer ES Plastiblend® ABS 8006 Availability: North AmericaForms: PelletsProcessing Method: Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 58.6 MPa @Thickness 3.20 mm |
8500 psi @Thickness 0.126 in |
Method I (3 point load), 2.0 mm/min, Injection Molded; ASTM D790 |
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp.. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | ASTM D790 |
Chase Plastics CP Pryme® A100HI ABS Molding Resin, High Impact Information provided by Chase Plastics. |
|||
Flexural Strength | 58.6 MPa | 8500 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® GPA300 ABS Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 58.6 - 86.2 MPa | 8500 - 12500 psi | |
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific .. |