Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790-95 |
Multibase Multi-Pro® 0505 RC Black 5.2% Glass Filled Polypropylene This product was specially designed for one customer's glass filled polypropylene application.Data provided by Multibase. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
Techmer ES HiFill FR® ABS GB10 FR 10% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
Techmer ES HiFill® PA6 0177 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 0146 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 0164 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
Techmer ES HiFill® PA6 0180 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers Centrex® 825 Sheet Extrusion Grade Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers SBS 2160 Clear Styrene Butadiene Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D-790 |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |