Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 380 MPa | 55100 psi | ISO 178 |
PolyOne OnForce™ LFT NN-30LCF/002 Grey Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Strength | 380 MPa | 55100 psi | ISO 178 |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA)
(Unverified Data**) Ixef GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without signi.. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
Lehmann & Voss LUVOCOM® 1-7488 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
MarkeTech Aluminum Oxide Ceramic - Alumina 96% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
MarkeTech Aluminum Oxide Ceramic - Alumina 97.5% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
MarkeTech Aluminum Oxide Ceramic - Alumina 98% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
GBC Grade 92 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
GBC Grade 96 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
GBC Grade 98 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
McDanel Advanced Ceramics 99.8% Alumina Information provided by McDanel Advanced Ceramic Technologies |
|||
Flexural Strength | 380 MPa @Temperature 22.0 °C |
55100 psi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |
|||
Flexural Strength | 380 MPa | 55100 psi | ISO 178 |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Flexural Strength | 380 MPa | 55100 psi | ISO 178 |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Flexural Strength | 380 MPa | 55100 psi | ISO 178 |
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Flexural Strength | 380 MPa | 55100 psi | ISO 178 |
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
Flexural Strength | 380 MPa | 55100 psi | DIN EN 843-1 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Flexural Strength | 380 MPa | 55100 psi | ISO 178 |
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Flexural Strength | 380 MPa | 55100 psi | |
Zircar Ceramics Alumina Furnaceware ZIRCAR Ceramics Alumina Furnaceware are high purity fully dense, fine grain aluminum oxide products suitable for use in applications with temperatures as high as 1800°C. Such uses include crucibles.. |
|||
Flexural Strength | 380 MPa @Diameter >=100 mm |
55100 psi @Diameter >=3.94 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Extremely good mechanical properties, at high temperatures. Low thermal conductivity.Applications: Material for components used in the aerospace industry. Insulation parts in wire weldi.. |
|||
Flexural Strength | 380 MPa | 55100 psi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Flexural Strength | 380 MPa @Temperature -40.0 °C |
55100 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Flexural Strength | 380 MPa @Temperature 23.0 °C |
55100 psi @Temperature 73.4 °F |
|
Ceradyne CeraTrex™ 146-IS Silicon Carbide Features:high puritycorrosion resistancewear resistanceApplications:semiconductor componentssputtering targetsInformation provided by Ceradyne Company |
|||
Flexural Strength | 380 MPa | 55100 psi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Flexural Strength | 380 MPa @Temperature 23.0 °C |
55100 psi @Temperature 73.4 °F |
Dry; EN2562 |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |
|||
Flexural Strength | 380 MPa | 55100 psi | ISO 178 |
Polyram Polytron A50B01 Nylon 6.6, 50% Long Fiber Glass 50% Long fiber glass reinforced black Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram. |