Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 300 MPa | 43500 psi | STN EN ISO 178 |
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant FeaturesModified homopolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfil.. |
|||
Flexural Strength | 300 MPa | 43500 psi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 60 Polyamide 6, 60% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 60% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Plastcom SLOVAMID 66 GF 50 LS PA66, 50% glass fibre, light stability FeaturesChemically reinforced with 50% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry, l.. |
|||
Flexural Strength | 300 MPa | 43500 psi | STN EN ISO 178 |
Plastcom SLOVAMID 66 GF 50 Polyamide 66, 50% Glass Fiber FeaturesChemically reinforced with 50% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Flexural Strength | 300 MPa | 43500 psi | ISO 178 |
PolyOne OnForce™ LFT NN-40LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Electrically conductive, suitable for continuous dischar.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Strength | 300 MPa | 43500 psi | ASTM D-790 |
Glastic GLASTHERM HT250 Insulation Sheet Glastherm Grade HT250 is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT250 is asbesto.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Misumi Alumina 96 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1/CF/20/TF/5 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Flexural Strength | 300 MPa | 43500 psi | |
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Flexural Strength | 300 MPa | 43500 psi | ISO 178 |
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Flexural Strength | 300 MPa | 43500 psi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Flexural Strength | 300 MPa | 43500 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP QC006I PA 6/10 LNP THERMOCOMPâ„¢ QC006I is a compound based on Nylon 6/10 containing 30% Carbon Fiber. Added features of this grade include: High Impact. |
|||
Flexural Strength | 300 MPa | 43500 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Flexural Strength | 300 MPa | 43500 psi | ASTM D790 |
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu.. |
|||
Flexural Strength | 300 MPa @Diameter >=100 mm |
43500 psi @Diameter >=3.94 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Mechanical and electrical applications. High mechanical strength. Self-extinguishing, halogen-free. Good resistance to chemicals.Information provided by Elektro-Isola |
|||
Flexural Strength | 300 MPa @Diameter >=100 mm |
43500 psi @Diameter >=3.94 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1 |
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Tubes Description: Mechanical and electrical applications. Arc-resistant and tracking-resistant material. Good flame resistance. Self-extinguishing. Halogen-free. Lower high-voltage values and insulation .. |
|||
Flexural Strength | >= 300 MPa @Diameter >=100 mm |
>= 43500 psi @Diameter >=3.94 in |
Perpendicular to laminations; IEC 1212-2 4.1 |
Hippe EP GC 22 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. High mechanical strength at elevated temperatures. Very good stability of .. |
|||
Flexural Strength | 300 MPa | 43500 psi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Flexural Strength | 300 MPa | 43500 psi | ISO 178 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
Flexural Strength | 300 MPa | 43500 psi | ISO 178 |
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli.. |
|||
Flexural Strength | 300 MPa @Temperature 23.0 °C |
43500 psi @Temperature 73.4 °F |
3.5% Strain; ISO 178 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |