Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 180 MPa | 26100 psi | STN EN ISO 178 |
Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Flexural Strength | 180 MPa | 26100 psi | ASTM D790 |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Flexural Strength | 180 MPa | 26100 psi | ASTM D790 |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Flexural Strength | 180 MPa | 26100 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
Flexural Strength | 180 MPa | 26100 psi | STN EN ISO 178 |
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |
|||
Flexural Strength | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Flexural Strength | 180 MPa | 26100 psi | ASTM D790 |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Strength | 180 MPa | 26100 psi | ASTM D790 |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Flexural Strength | 180 MPa | 26100 psi | ISO 178 |
Grupo Repol Dinalon® A1S25 G25PV0 25% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Flexural Strength | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Flexural Strength | 180 MPa | 26100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Flexural Strength | 180 MPa | 26100 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Flexural Strength | 180 MPa | 26100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East) VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage. |
|||
Flexural Strength | 180 MPa | 26100 psi | ISO 178 |
Polyplastics Duranex® 6300T Polybutylene Terephthalate (PBT), Low friction, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 180 MPa | 26100 psi | ISO 178 |
Polyram PlusTek PA320G3 Nylon 6.6 for Injection Molding, 15% Glass Fiber Reinforced, Flame Retardant 15% Glass fiber reinforced flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 180 MPa | 26100 psi | ISO 178 |
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in particular in the ABS system.. |
|||
Flexural Strength | 180 MPa | 26100 psi | ISO 178 |
Polyram Polytron P40N03 Polypropylene, 40% Long Glass Fibers Is a chemically coupled 40% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance ch.. |
|||
Flexural Strength | 180 MPa | 26100 psi | ISO 178-93 |
Wellman Wellamid® GSF25/15-66 22LH-N 40% Glass Sphere/Fiber Reinforced Nylon 66 Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 180 MPa | 26100 psi | ISO 178 |
Polyram RamSter PF305G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 180 MPa | 26100 psi | ASTM D790 |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Flexural Strength | >= 180 MPa @Diameter >=100 mm |
>= 26100 psi @Diameter >=3.94 in |
Perpendicular to laminations; IEC 1212-2 4.1 |
Hippe EP GC 42 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at elevated temperatures. Very good stability of electrical properties when exposed to high relative .. |
|||
Flexural Strength | 180 - 270 MPa | 26100 - 39200 psi | |
Alliance N-38SH Neodymium Iron Boron Magnetic Material |
|||
Flexural Strength | 180 - 270 MPa | 26100 - 39200 psi | |
Alliance N-33H Neodymium Iron Boron Magnetic Material |
|||
Flexural Strength | 180 - 270 MPa | 26100 - 39200 psi | |
Alliance N-38M Neodymium Iron Boron Magnetic Material |
|||
Flexural Strength | 180 - 270 MPa | 26100 - 39200 psi | |
Alliance N-33M Neodymium Iron Boron Magnetic Material |