Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Network Polymers NPP Nylon 66G13L Description: NylonInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Niche Polymer PPHG40BK Homopolymer PP, 40% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Strength | 148 MPa @Thickness 3.17 mm |
21500 psi @Thickness 0.125 in |
ASTM D790 |
PTS 15GFR-BK PBT- Flame Retardant, 15% Glass Filled PBT Black Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 148 MPa @Temperature 23.0 °C |
21500 psi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 148 MPa | 21500 psi | 2mm/min; ASTM D790 |
Kingfa JH-R0G30 Flame Retardant and 30% Glass Fiber Reinforced PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood processing propertiesApplications:Injection moldingAutomobile instrument panelCD-ROM base pick-upOA device an.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP EX00548C PEI LNP LUBRICOMP* EX00548C is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Clean Compounding System, Wear Resistant. |
|||
Flexural Strength | 148 MPa | 21500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Flexural Strength | 148 MPa | 21500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1520 compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D 790 |
SABIC Innovative Plastics Valox® DR48M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 148 MPa | 21500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Flexural Strength | 148 MPa | 21500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Flexural Strength | 148 MPa | 21500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 (Asia Pacific) LNP* STATKON* RFD03 is a compound based on PA 66 resin contaning Carbon Powder, Glass Fiber. Added features include: Electrically Conductive. |
|||
Flexural Strength | 148 MPa | 21500 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 4202-15 MFR Polycarbonate EMERGEâ„¢ PC 4202-15 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. A.. |
|||
Flexural Strength | 148 MPa | 21500 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 4202-8 MFR Polycarbonate EMERGEâ„¢ PC 4202-8 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. Ap.. |
|||
Flexural Strength | 148 MPa | 21500 psi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 5201-12 Polycarbonate Resin Overview: CALIBREâ„¢ 5201-12 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALI.. |
|||
Flexural Strength | 148 MPa | 21500 psi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 5201-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5201-8 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALIB.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Ensinger Tecapeek® XP-90 Compression Molded PEEK Compound, 25% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 148 MPa @Temperature -40.0 °C |
21500 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Applied Composites 8072 Polyester SMC Industry Application: TransportationProduct Application: AutomotiveDistinct Features: Zero Shrink, Superior Class A Finish, Improved Impact, Accepts Mold CoatingInformation provided by Applied Compo.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 515 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.10% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Applied Composites 120 Polyester SMC Industry Application: ElectricalProduct Application: Transmission ProductDistinct Features: Pigmentable UL 94 V-5, Stable @ 600 Hour QUV Accelerated Weather Testing, Passed 6 Mos. AZ Outdoor Weather.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Adell ER-38 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 148 MPa | 21500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF004L PES LNP* THERMOCOMP* JF004L is a compound is based on Polyethersulfone containing 20% Glass Fiber. Characteristics of this grade is: Low Extractible |