Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 125 MPa | 18100 psi | |
Plastcom SLOVAMID 6 FRC 3 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 for injection moulding with increased flammability resistance, with nonhalogen and phosporus flame retardant. Excellent.. |
|||
Flexural Strength | 125 MPa | 18100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Nemcon™ E-CPC/X1 Polycarbonate Alloy PC Alloy-ESD Range Electrical Conductivity with High HDT and improved processability.Information provided by Ovation Polymers |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Flexural Strength | <= 125 MPa | <= 18100 psi | ISO 178 |
Polykemi AB POLYfill PPH GF15030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
Perstorp Compounds Aminel FX Melamine Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp .. |
|||
Flexural Strength | 125 MPa | 18100 psi | |
Plastcom SLOVAMID 6 T 30 TS PA6, 30% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application. Increased modulus in tension - strength of the material. PA matrix reduction. PA for injection moulding with the content.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
Nilit FRIANYL A63 KV40 Nylon 6.6 for injection molding, 40% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 125 MPa | 18100 psi | |
Lehmann & Voss LUVOCOM® 1105-8174 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Flexural Strength | 125 MPa | 18100 psi | |
Lehmann & Voss LUVOCOM® 1105-7310 PEEK, with glass fiber, easy flowing, low-warpage Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High dimensionally stable precision parts, high continuous use temperature.Superheated ste.. |
|||
Flexural Strength | 125 MPa | 18100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3300 ULT Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral a.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Flexural Strength | 125 MPa | 18100 psi | 2mm/min; ISO 178 |
Teijin Panlite® GN-3410R Improved Mold Release, Glass Fiber Reinforced, Flame Resistant Polycarbonate Resin GF 10% reinforced, flame retardant and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machin.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Unitika AX-1500W Dry Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178-93 |
Wellman EcoLon® MR1660-BK 40% Mineral Reinforced Post Consumer Compound Nylon 66 Description: Mineral Reinforced Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178-93 |
Wellman Wellamid® MR409 22H-GY1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Gromax CCP PBT 3010-104 10% Glass Fiber Filled Product Description: PBT glass fiber 10% reinforced injection molding grade.Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent.. |
|||
Flexural Strength | 125 MPa | 18100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Flexural Strength | 125 MPa | 18100 psi | 3.5%; ISO 178 |
GEHR Plastics PPE-30GF Polyphenylene Ether, 30% Glass Fiber
(discontinued **) The 30% glass fiber reinforced PPE has an improved dimensional stability, a very high stiffness and heat resistance that allows further uses. |