Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 84.0 MPa | <= 12200 psi | ISO 178 |
Polykemi AB POLYabs N20 ABS Information provided by Polykemi AB |
|||
Flexural Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ A3525 ASA+PC Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics Lexan® LCR200 PBT+PC (Asia Pacific) |
|||
Flexural Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific) LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific) LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Kotec Carbotex K-30FR Polycarbonate, Flame Retardant Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Kotec Carbotex KFR-30 Polycarbonate, Flame Retardant Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Kotec Carbotex KFR-30T12 Polycarbonate, Flame Retardant Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific) LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1000 PC (Asia Pacific) |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66 LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific) LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX93500 PC LNP STAT-KON* DX93500 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D 790 |
SABIC Innovative Plastics Valox® VAC3001 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS LNP* STAT-LOY* N30009 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Flexural Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Styron Pulse® 2000 ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX91077 PC LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS (Asia Pacific) LNP STAT-LOY* NX03583 is a compound based on PC+ABS Blend resin containing Anti-Static, Flame Retardant. Added features of this material include: Antistat. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX6009 PPE+PS+PA6 (Asia Pacific) PA6 based unfilled GTX for Wheel cover |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Plenco 1508 Polyester, Briquette, Transfer Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Plenco 4485 Phenolic, Granular, Injection Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Unitika P-3001S Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
Polyplastics Duracon® ES-5 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
Polyplastics Duranex® 601SA Polybutylene Terephthalate (PBT), Low density, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Chase Plastics CP Pryme® N213GL (COND, 50% RH) Nylon 6, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |