Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 76.5 MPa | 11100 psi | ASTM D790 |
PolyOne Geon™ HTX 92052 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Flexural Strength | 76.5 MPa | 11100 psi | ASTM D790 |
Techmer ES Plastiblend® ABS 8011 Availability: North AmericaForms: PelletsFeatures: PlatableInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | ASTM D 790 |
Styrolution PS 3600/3601 GPPS Exceptional flow characteristicsGood for thin wall and complex partsUSP Class VI certifiedInformation provided by Styrolution |
|||
Flexural Strength | 76.5 MPa | 11100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | Method I (3 point load), 1.3 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | Method I (3 point load), 1.3 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Flexural Strength | 76.5 MPa @Thickness 3.20 mm |
11100 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 203 LV General Purpose Polystyrene CharacteristicsGood flow grade with good mechanical properties Good clarity and flexibility Easy processing grade and suitable for thin walled applicationsProcessing Extrusion MoldingApplicationsSu.. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | ASTM D790 |
Chase Plastics CP Pryme® A100 ABS Molding Resin Information provided by Chase Plastics. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | ASTM D790 |
Daelim H&L Plavis-MS DF MoS2 Filled Aromatic Polyimide Bearing Direct Formed. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the criti.. |
|||
Flexural Strength | 76.52 MPa | 11100 psi | ASTM D790 |
E-Polymers TEKAMID® H14HT High Toughness PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | ASTM D-790 |
Axiall HHP-190 Rigid PVC, Extrusion Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi.. |
|||
Flexural Strength | 76.5 MPa | 11100 psi | ASTM D-790 |
Axiall 9153 Rigid PVC, Molding Georgia Gulf 9153 is an excellent combination of chemical resistance, impact and processing for chemically active products, such as pine oil cleaners.Information provided by Georgia GulfGeorgia Gulf.. |