Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 82.7 - 103 MPa | 12000 - 14900 psi | ASTM D790 |
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne |
|||
Flexural Strength | 89.6 - 103 MPa | 13000 - 14900 psi | ASTM D790 |
PolyOne Stat-Tech™ PC-CB2/000 CR Polycarbonate (PC) Stat-Tech™ PC-CB2/000 CR XP100827Information provided by PolyOne |
|||
Flexural Strength | 68.9 - 103 MPa | 10000 - 15000 psi | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |