Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Niche Polymer PCM18BK PC Information provided by Niche Polymer |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Polymer Resources PC-UV3-D-[color]-1 Polycarbonate, UV-stabilized, High Flow with Mold Release Polycarbonate, UV-stabilized, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | after 16 hours in 50°C water |
Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler Product data demonstrates the effect of the Novakup (lamellar quartz surface treated with 0.5% A-1100) filler. A separate entry demonstrates the effect of untreated Novacite filler in thermopla.. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Techmer ES Statiblend® POM CO Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeature: ConductiveTPCI# 9962114Information provided by TP Composites, Inc. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Chase Plastics CP Pryme® NN113GL (COND, 50% RH) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Entec Hylex® P1017L1 HB Polycarbonate Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Clear/Transparent Information provided by Entec |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Entec Hylex® P1017L2 HB Polycarbonate Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Blue Information provided by Entec |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Entec Hylex® P1317L1 HB Polycarbonate UV Stabilized, Higher Flow, Mold Release, Water ClearInformation provided by Entec. |
|||
Flexural Strength | 95.8 MPa @Temperature 150 °C |
13900 psi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |
|||
Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
Techmer ES HiFill FR® PBT 0166 B FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |