Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ A6020 ASA+PC Available in North America Features: Good Impact Resistance and High Heat Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E1500 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7001 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7001 is 27-29; Geon E7456 is 40-49; Geon E7130 is 38-43; Geon E7370 is 26-31Information provided by PolyOne |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
PolyOne Edgetek® XT XT-500-CX01 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 409 L MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | |
SGL Carbon Group Ridurid® V 1017 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 79.3 MPa @Temperature 23.0 °C |
11500 psi @Temperature 73.4 °F |
2; ISO 178 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Electrablend® PC 04003 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Plastics Group Polifil® 625L Nylon 6/6 (DAM) Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group... |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Chase Plastics CP Pryme® A100HF ABS Molding Resin, High Flow Information provided by Chase Plastics. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Chase Plastics CP Pryme® AC300 Acetal Copolymer, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | ASTM D-790 |
Axiall 9209 Rigid PVC, Molding Georgia Gulf 9209 is a food grade compound containing excellent optical and processing characteristics. It is suitable for use in a variety of food, cosmetic and general purpose packaging applicati.. |
|||
Flexural Strength | 79.3 MPa | 11500 psi | for Epoxy Coating |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Flexural Strength | 79.3 - 107 MPa | 11500 - 15500 psi | |
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound BMC T10(GP) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T10(GP) is well suited for injection, transfer or compression molding of intricate parts... |