Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 60.0 MPa | 8700 psi | STN EN ISO 178 |
Plastcom SLOVAMID 66 HI Polyamide 66, Impact Grade FeaturesModified with thermoplastic reactive elastomer, determined for mouldings with high toughness also at low temperatures. Eligible application for ski-shoes, helmets for sport and other safety.. |
|||
Flexural Strength | 60.0 - 70.0 MPa | 8700 - 10200 psi | ASTM D790-03 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | STN EN ISO 178 |
Plastcom SLOVAMID 6 HI-M PA6 with improved impact strength PA 6 with the content of thermoplastic elastomer. Impacted, for moldings with higher toughness even at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets, protecti.. |
|||
Flexural Strength | <= 60.0 MPa | <= 8700 psi | ISO 178 |
Polykemi AB POLYfill PPH Q15030 E10 Polypropylene Homopolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ASTM D790 |
PolyOne Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
NOVA Chemicals DYLARK® 250 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America.. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | after 16 hours in 50°C water |
Malvern Minerals Thermoplastic Polyester with Novacite® 1250 Quartz Filler Product data demonstrates the effect of the Novacite (untreated lamellar quartz) filler. A separate entry demonstrates the effect of surface-treated Novakup filler in thermoplastic polyester Th.. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | 2mm/min; ASTM D790 |
Kingfa HF-618 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ASTM D790 |
Kolon KOCETAL® EL304 Toughened Grade Acetal Resin Flexible grade. Applications: Flexible products. Information provided by API-Kolon. |
|||
Flexural Strength | 60.0 MPa @Temperature 22.0 °C |
8700 psi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of .. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | 5 mm/min; ISO 178 |
Gromax BTE70-FN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | 5 mm/min; ISO 178 |
Gromax BTE90-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
Kuraray Genestarâ„¢ N1006D-H31 Nylon Standard unreinforced extrusion grade. Main Features:Chemical resistanceLong term heat resistanceExample of applications:Tube applications |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
Styrolution Novodur® E401 ABS Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ASTM-D790 |
Polyram RamLloy PVB101 ABS/NYLON alloy, Impact Modified Impact modified ABS/NYLON alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ISO 178-93 |
Wellman Wellamid® XT1482-WT1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ASTM-D790 |
Polyram RamTal PM8427 Acetal, Impact modified Impact modified polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ASTM D790 |
Plenco 6310 Phenolic, Granular, Compression Molded PLENCO 06310 is a glass and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. 06310 is available in black.Information supplied by Plenco. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | cond; ISO 178 |
DSM Novamid® 1010GN7-20 BK37 PA6-GF20 FR(30) 0 20% Glass Reinforced, Flame Retardant, Halogen free |
|||
Flexural Strength | 60.0 MPa | 8700 psi | dry; ISO 178 |
DSM Novamid® ST120 NAT PA6-I Impact Modified, Injection Molding |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
Denka TE-30 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 60.0 MPa @Thickness 3.17 mm |
8700 psi @Thickness 0.125 in |
chs 0.05 in/min; 2 in span; ASTM D790 |
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a.. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | |
Advanced Ceramics ACL 2089 Cordierite Cordierite glass-ceramic has good thermal shock properties and is suitable for heat resistant components which undergo rapid thermal cycling.Information provided by Advanced Ceramics Limited (ACL) |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436G20CL Glass Reinforced |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N2300STHL BK Post Consumer Recycle Nylon 6 Superior Toughness, Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific) LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
Lucite International Diakon® ST45G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |