Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 230 MPa | 33400 psi | ISO 178 |
PolyOne OnForce™ LFT SF-40LCF/000 Black Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178 |
PolyOne Nymax™ ND 1233 GF Black Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Strength | 230 MPa | 33400 psi | STN EN ISO 178 |
Plastcom SLOVAMID 6 NG GF 30 Polyamide 6, 30% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Flexural Strength | <= 230 MPa | <= 33400 psi | ISO 178 |
Polykemi AB SCANMID 6 B22^ E F40 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Flexural Strength | 230 MPa | 33400 psi | |
Lehmann & Voss LUVOCOM® 1-7882 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM D790 |
Kuraray Genestarâ„¢ G1350H Nylon, 35% Glass Filled Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in .. |
|||
Flexural Strength | 230 MPa | 33400 psi | |
Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2mm/min; ASTM D790 |
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose) Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Flexural Strength | 230 MPa | 33400 psi | |
SPS Guang Zhou PONYLâ„¢ 4001G30 GF30%-PA66 Characteristic: High mechanical properties, superior heat resistance, good dimensional stabilityApplications: Power tool, chassis and E/E partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66 LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Europe-Africa-Middle East) UV stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC003 PA 66 (Europe-Africa-Middle East) 15% carbon fibre reinforced Polyamide 66 injection moulding resin. |
|||
Flexural Strength | 230 MPa | 33300 psi | ASTM D790 |
Chase Plastics CP Pryme® NN130GMD2HS (COND, 50% RH) Nylon 66, 30% Glass Fiber Reinforced, 2% MoS2 Lubricated, Heat Stabilized Information provided by Chase Plastics. |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM-D790 |
Polyram Polytron P60B01 Homopolymer Polypropylene, Chemically Coupled 60% LGF A chemically coupled 60% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178-93 |
Wellman Wellamid® GF33-66 XE-BKDX9 33% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178 |
Polyram PlusTek PB300G4 Nylon 6 for Injection Molding, 20% Glass-Fiber Reinforced 20% Glass fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 230 MPa | 33400 psi | cond; ISO 178 |
DSM Novamid® 1013GH45 1 NA/BK701 PA6-GF45 45% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide BG6U PA6, 30% Glass Fiber Filled, UV Stabilized, Injection Molded Staramide BG6U is an UV Stabilized, 30% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide BG6 PA6, 30% Glass Filled, Injection Molded BG6 is a 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Dry, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Strength | 230 MPa | 33400 psi | |
Plastcom SLOVAMID 6 NG GF 30 LS PA6, 30% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |