Polymer Property : Tensile Stress = 2710 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 18.7 MPa

@Strain 0.270 %,
Temperature 90.0 °C
2710 psi

@Strain 0.270 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 18.7 MPa

@Strain 0.270 %,
Temperature 90.0 °C
2710 psi

@Strain 0.270 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)  (Unverified Data**)
45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Tensile Stress 18.7 MPa

@Strain 0.500 %,
Temperature -40.0 °C
2710 psi

@Strain 0.500 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring ..
Tensile Stress 18.7 MPa

@Strain 0.500 %,
Temperature -40.0 °C
2710 psi

@Strain 0.500 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear ..
Tensile Stress 18.7 MPa

@Strain 8.56 %,
Temperature 40.0 °C
2710 psi

@Strain 8.56 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 18.7 MPa

@Strain 1.99 %,
Temperature 150 °C
2710 psi

@Strain 1.99 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per..
Tensile Stress 18.7 MPa

@Strain 10.0 %,
Temperature 0.000 °C
2710 psi

@Strain 10.0 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..