Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.0 MPa @Strain 1.00 %, Temperature 120 °C |
1740 psi @Strain 1.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 12.0 MPa @Strain 1.00 %, Temperature 160 °C |
1740 psi @Strain 1.00 %, Temperature 320 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 12.0 MPa @Strain 2.00 %, Temperature 200 °C |
1740 psi @Strain 2.00 %, Temperature 392 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 12.0 MPa @Strain 3.00 %, Temperature 230 °C |
1740 psi @Strain 3.00 %, Temperature 446 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 12.0 MPa @Strain 5.00 % |
1740 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 5.00 % |
1740 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 117.82 %, Temperature 120 °C |
1740 psi @Strain 117.82 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 0.528 %, Time 3.60e+6 sec |
1740 psi @Strain 0.528 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.443 %, Time 36000 sec |
1740 psi @Strain 0.443 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.403 %, Time 3600 sec |
1740 psi @Strain 0.403 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.100 %, Temperature 23.0 °C |
1740 psi @Strain 0.100 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.600 %, Temperature -20.0 °C |
1740 psi @Strain 0.600 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Tensile Stress | 12.0 MPa @Strain 5.00 %, Temperature 23.0 °C |
1740 psi @Strain 5.00 %, Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 12.0 MPa @Strain 5.00 % |
1740 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 50.0 % |
1740 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 1.52 %, Time 360000 sec |
1740 psi @Strain 1.52 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 1.45 %, Time 3.60e+7 sec |
1740 psi @Strain 1.45 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.656 %, Time 3600 sec |
1740 psi @Strain 0.656 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.947 %, Time 360000 sec |
1740 psi @Strain 0.947 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 12.0 MPa @Strain 2.91667 %, Time 3.60e+7 sec |
1740 psi @Strain 2.91667 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 2.275 %, Time 3.60e+6 sec |
1740 psi @Strain 2.275 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Time 3600 sec, Strain 1.19 % |
1740 psi @Time 1.00 hour, Strain 1.19 % |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | >= 12.0 MPa @Strain 300 % |
>= 1740 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 485A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | >= 12.0 MPa @Strain 300 % |
>= 1740 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 790A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Stress | 12.0 MPa @Strain 0.100 %, Temperature 23.0 °C |
1740 psi @Strain 0.100 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 10.0 %, Time 3.60e+6 sec |
1740 psi @Strain 10.0 %, Time 1000 hour |
100°C; ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Tensile Stress | 12.0 MPa @Strain 5.00 %, Time 3.60e+6 sec |
1740 psi @Strain 5.00 %, Time 1000 hour |
60°C; ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |