Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 69.5 MPa @Strain 2.41 %, Temperature 40.0 °C |
10100 psi @Strain 2.41 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Stress | 69.7 MPa @Strain 3.00 %, Temperature 90.0 °C |
10100 psi @Strain 3.00 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Tensile Stress | 69.9 MPa @Strain 6.20 %, Temperature 23.0 °C |
10100 psi @Strain 6.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Tensile Stress | 69.9 MPa @Strain 6.20 %, Temperature 23.0 °C |
10100 psi @Strain 6.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Tensile Stress | 69.61 MPa @Strain 1.25 %, Temperature 23.0 °C |
10100 psi @Strain 1.25 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66 + Nylon 6
(Unverified Data**) 35% Glass Reinforced Polyamide 66 Developed for Electrical and Electronics ApplicationsZytel 70G35EF NC010 is a 35% glass reinforced polyamide 66 developed for electrical and electronics application.. |
|||
Tensile Stress | 69.61 MPa @Strain 1.25 %, Temperature 23.0 °C |
10100 psi @Strain 1.25 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSL NC010 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL NC010 is a 35% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Tensile Stress | 69.8 MPa @Strain 1.12 %, Temperature 23.0 °C |
10100 psi @Strain 1.12 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G35HSLRA4 BK267 is a 35% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection m.. |
|||
Tensile Stress | 69.5 MPa @Strain 0.760 %, Temperature 0.000 °C |
10100 psi @Strain 0.760 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo.. |
|||
Tensile Stress | 69.3 MPa @Strain 1.03 %, Temperature 0.000 °C |
10100 psi @Strain 1.03 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Tensile Stress | 69.9 MPa @Strain 3.39 %, Temperature 180 °C |
10100 psi @Strain 3.39 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc.. |
|||
Tensile Stress | 69.9 MPa @Strain 3.85 %, Temperature 90.0 °C |
10100 psi @Strain 3.85 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |