Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 40.0 MPa @Strain 7.60 %, Temperature 40.0 °C |
5800 psi @Strain 7.60 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 40.0 MPa @Strain 2.31 %, Temperature -20.0 °C |
5800 psi @Strain 2.31 %, Temperature -4.00 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 40.0 MPa @Strain 1.00 %, Temperature 80.0 °C |
5800 psi @Strain 1.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Stress | 40.0 MPa @Strain 2.00 %, Temperature 150 °C |
5800 psi @Strain 2.00 %, Temperature 302 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Stress | 40.0 MPa @Strain 1.00 %, Temperature 80.0 °C |
5800 psi @Strain 1.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Stress | 40.0 MPa @Strain 1.00 %, Temperature 100 °C |
5800 psi @Strain 1.00 %, Temperature 212 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 40.0 MPa @Strain 1.00 %, Temperature 150 °C |
5800 psi @Strain 1.00 %, Temperature 302 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 40.0 MPa @Strain 5.00 % |
5800 psi @Strain 5.00 % |
|
Solvay TECHNYL® A 221 PA66, Conditioned Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Tensile Stress | 40.0 MPa @Strain 6.00 %, Temperature 120 °C |
5800 psi @Strain 6.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 40.0 MPa @Strain 20.0 %, Temperature 23.0 °C |
5800 psi @Strain 20.0 %, Temperature 73.4 °F |
|
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Tensile Stress | 40.0 MPa @Strain 1.75 %, Time 3.60e+6 sec |
5800 psi @Strain 1.75 %, Time 1000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 40.0 MPa @Strain 1.17 %, Time 36000 sec |
5800 psi @Strain 1.17 %, Time 10.0 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 40.0 MPa @Strain 2.30 %, Temperature -20.0 °C |
5800 psi @Strain 2.30 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 40.0 MPa @Strain 7.00 %, Temperature 150 °C |
5800 psi @Strain 7.00 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Tensile Stress | 40.0 MPa @Strain 1.01 %, Temperature 150 °C |
5800 psi @Strain 1.01 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |
|||
Tensile Stress | 40.0 MPa @Strain 300 % |
5800 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer Zythane™ 4065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 40.0 MPa @Strain 5.00 %, Temperature 140 °C |
5800 psi @Strain 5.00 %, Temperature 284 °F |
ISO 527 |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 40.0 MPa @Temperature 150 °C |
5800 psi @Temperature 302 °F |
|
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand .. |
|||
Tensile Stress | 40.0 MPa @Temperature 220 °C |
5800 psi @Temperature 428 °F |
|
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand .. |
|||
Tensile Stress | 40.0 MPa @Strain 0.624 %, Time 360000 sec |
5800 psi @Strain 0.624 %, Time 100 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Tensile Stress | 40.0 MPa @Strain 0.537 %, Time 36000 sec |
5800 psi @Strain 0.537 %, Time 10.0 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Tensile Stress | 40.0 MPa @Strain 0.489 %, Time 3600 sec |
5800 psi @Strain 0.489 %, Time 1.00 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Tensile Stress | 40.0 MPa @Strain 0.921 %, Time 3.60e+7 sec |
5800 psi @Strain 0.921 %, Time 10000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Tensile Stress | 40.0 MPa @Strain 0.870 %, Time 1.80e+7 sec |
5800 psi @Strain 0.870 %, Time 5000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Tensile Stress | 40.0 MPa @Strain 0.749 %, Time 3.60e+6 sec |
5800 psi @Strain 0.749 %, Time 1000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Tensile Stress | 40.0 MPa @Strain 2.00 %, Temperature 30.0 °C |
5800 psi @Strain 2.00 %, Temperature 86.0 °F |
ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Tensile Stress | 40.0 MPa @Strain 0.500 %, Temperature 40.0 °C |
5800 psi @Strain 0.500 %, Temperature 104 °F |
ISO 527 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 40.0 MPa @Strain 2.00 %, Temperature 140 °C |
5800 psi @Strain 2.00 %, Temperature 284 °F |
ISO 527 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 40.0 MPa @Strain 3.00 %, Time 3.60e+6 sec |
5800 psi @Strain 3.00 %, Time 1000 hour |
100°C; DIN 50014-23/50-2 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 40.0 MPa @Strain 0.600 %, Time 3.60e+6 sec |
5800 psi @Strain 0.600 %, Time 1000 hour |
DIN 50014-23/50-2 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |