Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 197 GPa @Temperature 400 °C |
28600 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 400 °C |
28600 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 200 °C |
28600 ksi @Temperature 392 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, 1.6 mm sheet Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, aged 1000 hours at 316°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, aged 1000 hours at 982°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, all-weld metal, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, mill annealed Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, plate, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 427 °C |
28600 ksi @Temperature 801 °F |
(heat treated at 1121°C (2050°F), water quenched plate) |
Haynes Ultimet® alloy, plate, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 400 °C |
28600 ksi @Temperature 752 °F |
Dynamic |
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 400 °C |
28600 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 400 °C |
28600 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 400 °C |
28600 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 20.0 °C |
28600 ksi @Temperature 68.0 °F |
|
EDRO #7 Shock Resistant S7 Tool Steel EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 400 °C |
28600 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Modulus of Elasticity | 197 GPa @Temperature 400 °C |
28600 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |