Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.54 J/cm @Temperature 22.8 °C |
16.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Izod Impact, Notched | 8.54 J/cm @Temperature 22.8 °C |
16.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Izod Impact, Notched | 8.54 J/cm @Temperature 22.8 °C |
16.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC/PBT-1830 Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PC E IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact Modified and High ViscosityProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PC IM X Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Mold ReleaseFeatures: Impact Modified and Good Mold ReleaseProcessing Method: Injection MoldingInformation provided by TP Compo.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PET IM 1016 UV Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM L UV Nylon 66 Availability: North AmericaForms: PelletsAdditive: UV Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PC IM Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Notched | 8.54 J/cm @Temperature 22.8 °C |
16.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 8.54 J/cm @Temperature 22.8 °C |
16.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm, Temperature 22.2 °C |
16.0 ft-lb/in @Thickness 0.125 in, Temperature 72.0 °F |
ASTM D-256 |
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
16.0 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 7055 Rigid PVC, Extrusion Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat.. |