Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® PC/PET IM 1016 UV

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Techmer ES Plastiblend® PC/PET IM 1016 UV.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.17 %

@Time 86400 sec
0.17 %

@Time 24.0 hour
ASTM D570
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 265 °C
12 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
28 g/10 min

@Load 2.16 kg,
Temperature 285 °C
28 g/10 min

@Load 4.76 lb,
Temperature 545 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Yield 53.8 MPa
7800 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Flexural Yield Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
12.0 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Dart Drop, Total Energy 5.14 J

@Temperature -40.0 °C
3.79 ft-lb

@Temperature -40.0 °F
ASTM D3763
5.31 J

@Temperature 22.8 °C
3.92 ft-lb

@Temperature 73.0 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
35.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
240 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+15 ohm-cm
7.00e+15 ohm-cm
ASTM D257
Dielectric Strength 27.6 kV/mm
700 kV/in
Method A (Short-Time); ASTM D149