Mechanical Properties Metric English Comments
Izod Impact, Notched 0.588 J/cm

@Temperature -20.0 °C
1.10 ft-lb/in

@Temperature -4.00 °F
ASTM D256
PolyMirae Moplen EP400M Injection Molding Grade Polypropylene
Moplen EP400M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP400M is a block copolymer selected by customers for use in in..
Izod Impact, Notched 0.588 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.10 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical ALPHALAC SG910 HIPS
High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA..
Izod Impact, Notched 0.588 J/cm

@Thickness 6.50 mm,
Temperature -30.0 °C
1.10 ft-lb/in

@Thickness 0.256 in,
Temperature -22.0 °F
ASTM D256
LG Chemical ALPHALAC SH860 HIPS
Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical
Izod Impact, Notched 0.588 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LI970HF Co-Extrusion ASA
Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical
Izod Impact, Notched 0.588 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose
Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
Izod Impact, Notched 0.588 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMIPLAS LD590 Light diffusion ABS
Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical
Izod Impact, Notched >= 0.588 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
>= 1.10 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOL GP3202 PP+MF20%
Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG..
Izod Impact, Notched >= 0.588 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
>= 1.10 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOL GP3202B PP+MF20%
Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Izod Impact, Notched >= 0.588 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
>= 1.10 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOL GP3202Z PP+MF20%
Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.588 J/cm

@Thickness 6.35 mm
1.10 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.588 J/cm

@Temperature 0.000 °C
1.10 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SCG Chemicals EL-Proâ„¢ P642J Polypropylene Injection Molding
Key Characteristics:Good flowabilityExcellent stiffnessHigh impact strengthMechanical property balanceContains UV stabilizer and anti-static agentRecommended Applications:Industrial and household pr..
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin
NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Izod Impact, Notched 0.587 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Dow R131-02A Polypropylene Random Copolymer Resin
DOW R131-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier..
Izod Impact, Notched 0.587 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Dow R132-02A Polypropylene Random Copolymer Resin
DOW R132-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier..
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall NR-5009 Rigid PVC, Molding
Georgia Gulf NR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent processability, ..
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
Axiall SP-7107 Rigid PVC, Molding
Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it ..
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall MD-5009 Rigid PVC, Molding
Georgia Gulf MD-5009 is a rigid, fitting-grade PVC compound designed for hot spruce/runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, whi..
Izod Impact, Notched 0.588 J/cm

@Thickness 6.40 mm
1.10 ft-lb/in

@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IMG1120 Glass Reinforced Grade
Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali
Izod Impact, Notched 0.587 J/cm

@Temperature -18.0 °C
1.10 ft-lb/in

@Temperature -0.400 °F
ASTM D256
Formosa Plastics Formolene® 6620A Impact Copolymer Polypropylene
High Impact Copolymer for Injection Molding Formolene® 6620A is a copolymer of polypropylene designed and formulated for injection molding applications including pails, crates and furniture. It con..
Izod Impact, Notched 0.587 J/cm

@Temperature -18.0 °C
1.10 ft-lb/in

@Temperature -0.400 °F
ASTM D256
Formosa Plastics Formolene® 6630A Impact Copolymer Polypropylene
Impact Copolymer for Injection Molding Applications Formolene® 6630A is a high impact copolymer of polypropylene designed and formulated for injection-molded applications. It contains a unique comb..
Izod Impact, Notched 0.588 J/cm

@Thickness 3.20 mm
1.10 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron IMGS20 Glass Reinforced Grade
Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali
Izod Impact, Notched 0.588 J/cm

@Temperature 0.000 °C
1.10 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding
Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical ..