Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 1820 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1820 engineered polyolefin is designed for automotive exterior applications that require energy management combined with excellent ductility and stiffness over a broad temperat.. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial, @ ULT, deflection = 14 mm; ASTM D 3763 |
Total Finathene® WR 201 B N HDPE blow molding
(discontinued **) FINATHENE® WR 201 B N is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® WR 201 B N has been developed for the blow molding of Plastic Fuel .. |
|||
Impact Test | 20.0 J @Temperature 5.00 °C |
14.8 ft-lb @Temperature 41.0 °F |
Montell drop weight impact strength |
LyondellBasell Pro-fax SD242 Polypropylene Impact Copolymer Key Features: short cycle times for high productivity, good cold impact resistance, good stiffness and impact balance, high flow ease of mold filling and minimum warpage, low odor and low taste tran.. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
LyondellBasell DEXFLEX® 727 TPO Description: DEXFLEX® 727 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, good low-temperature impact resistance.. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp DP0039 PC LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing 45% Glass Fiber. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl HIPS3191 PS This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Impact Test | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp 2FL24 FP-E (EFTE) LNP* 2FL24 is a Fluoropolymer, ETFE grade containing Glass Fibers and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 (Asia Pacific) LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Impact Test | 20.0 J @Temperature 0.000 °C |
14.8 ft-lb @Temperature 32.0 °F |
Total Penetration Energy; ISO 6603-2 |
Borealis Borpact™ SE920MO Polypropylene Homopolymer for Injection Molding Borpact SE920MO is a high impact and transparent polypropylene. Borpact SE920MO is a new generation polypropylene having properties that were earlier not possible to combine. Borpact SE920MO offers.. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | During tempering at 250°C tempering temperature (2h + 2h) |
Assab Steels 8407 2M Hot Work Steel ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform .. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | tempering temperature 400°C. Austenitizing temperature 1020°C. |
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Impact Test | >= 20.0 J | >= 14.8 ft-lb | |
Assab Steels 705M Machinery Steel ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil harde.. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers DEXPRO® R120 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R120 is a reactor-grade thermoplastic elastomeric olefin resin with a good balance of impact performance, stiffness, and paintability. Applications: Painted bumper fasciasInfor.. |
|||
Impact Test | 20.0 J | 14.8 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers DEXFLEX® D160HS TPO
(discontinued **) Description: DEXFLEX® D160HS is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require excellent durability, low-temperature impact resistance, low ther.. |