Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 260 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.79 - 3.24 GPa
260 - 470 ksi
Average value: 2.37 GPa Grade Count:27
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Modulus of Elasticity 1.79 - 3.10 GPa
260 - 450 ksi
Average value: 2.68 GPa Grade Count:16
Overview of materials for Chlorinated PVC (CPVC)
This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 1.79 - 36.5 GPa
260 - 5290 ksi
Average value: 4.98 GPa Grade Count:78
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Modulus of Elasticity 1.79 GPa
260 ksi
ASTM D638
Total PPH 3720WZ Polypropylene, Injection Molding Grade
High flow reactor injection molding homopolymerHigh Flow - FINA 3720WZ has high flow characteristics that result in ease of filling thin wall parts.Nucleation - FINA 3720WZ is nucleated to provide f..
Modulus of Elasticity 1.79 GPa
260 ksi
ASTM D638
Total PPH 3721WZ Polypropylene, Injection Molding Grade
High flow reactor homopolymer with a high level of antistatHigh Flow - FINA 3721WZ is designed with high flow characteristics for ease of filling thin wall parts.High Antistat - FINA 3721WZ is engin..
Modulus of Elasticity 1.79 GPa
260 ksi
ASTM D638
Total PPH 3925WZ Polypropylene, Injection Molding Grade
Easy flow injection molding homopolymerNucleation - FINA 3925WZ is nucleated to provide fast cycle time and improve contact clarity.Antistat - FINA 3925WZ contains an antistat that will help protect..
Modulus of Elasticity 1.79 GPa
260 ksi
IPC TM-650 2.4.18.3
Arlon CLTE-AT Commercial Ceramic PTFE
Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing ..
Modulus of Elasticity 1.79 GPa
260 ksi
IPC TM-650 2.4.18.3
Arlon CLTE-XT High Precision Ceramic PTFE
Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing ..
Modulus of Elasticity 1.79 - 3.45 GPa
260 - 500 ksi
Average value: 2.77 GPa Grade Count:9
Overview of materials for Acrylic, UV Stabilized, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of..
Copyright © lookpolymers.com All Rights Reserved