Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 7.58 GPa | 1100 ksi | ASTM D638 |
Technetics Group Amicon™ PEEK 30% Carbon
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Modulus of Elasticity | 7.58 - 8.96 GPa | 1100 - 1300 ksi | ASTM D638 |
Premix Premi-Glas® 1201-10 Polyester SMC
(discontinued **) Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
Modulus of Elasticity | 7.60 - 21.0 GPa | 1100 - 3050 ksi | Average value: 11.1 GPa Grade Count:7 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 7.60 - 9.40 GPa | 1100 - 1360 ksi | Average value: 8.40 GPa Grade Count:25 |
Overview of materials for Phenolic, Novolac, Woodflour Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 7.58 - 13.3 GPa | 1100 - 1930 ksi | Average value: 9.64 GPa Grade Count:8 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Modulus of Elasticity | 7.58 GPa | 1100 ksi | |
SGL Carbon Group Ridurid® V 1352 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 7.58 GPa | 1100 ksi | ASTM D638 |
Techmer ES Electrafil® J-50/CF/10 Polycarbonate, 10% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Modulus of Elasticity | 7.58 - 18.6 GPa | 1100 - 2700 ksi | Average value: 12.1 GPa Grade Count:79 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |