Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 9.50 - 30.0 GPa | 1380 - 4350 ksi | Average value: 18.7 GPa Grade Count:19 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 1105-8053/EM/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 50-0833 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Electrical.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 50-8025 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 6-7433 Polyamide 12, with carbon fiber, hydrolysis resistant Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15 Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/SI/2-2 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 1105-7720/BE PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® PC-50/GF/30/TF/15/ BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | ISO 527-2 |
Tisan TISESTER® 30% Glass Fiber Reinforced and heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | ISO 527-2 |
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | ISO 527-2 |
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | ISO 527 |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | ISO 527 |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | ISO 527-2 |
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | ISO 527 |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | ISO 527 |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |
|||
Modulus of Elasticity | 9.50 GPa | 1380 ksi | |
Lehmann & Voss LUVOCOM® 1105-7173/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |