Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HF1110 PC General purpose grade. Good clarity, heat resistance, property retention and dimensional stability. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HF1130R PC PC, High Flow, Mold Release, UV-Stabilized |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HF1140R PC (Asia Pacific) LEXAN HF1140R is a high flow grade. This material is especially designed for applications that require thin wall sections and high flow lengths. FDA food contact compliant in limited colors. Effe.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LSHF PC (Europe-Africa-Middle East) Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HF1110R PC (Asia Pacific) High flow grade. Easy mold release version of LEXAN HF1110. For thin wall lighting lenses, data storage components and safety eyewear lenses. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HF1130 PC UV-stabilized. Good clarity, heat resistance, property retention and dimensional stability. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HF1130 PC (Asia Pacific) UV-stabilized. Good clarity, heat resistance, property retention and dimensional stability. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HF1140 PC Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HF1140 PC (Europe-Africa-Middle East) Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Tensile Impact Strength | 378 - 631 kJ/m² | 180 - 300 ft-lb/in² | Average value: 498 kJ/m² Grade Count:16 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Tensile Impact Strength | 378 - 589 kJ/m² | 180 - 280 ft-lb/in² | Average value: 541 kJ/m² Grade Count:6 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM Data |
Styron CALIBRE™ 200 22 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM D1822, Type S |
Styron CALIBREâ„¢ 201-22 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Resin Overview: CALIBREâ„¢ 201-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 2061 HD 15 Polycarbonate Resin Overview: CALIBREâ„¢ 2061 HD 15 Polycarbonate Resins are designed for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061 HD 15 Polycarbonate Resins offer a .. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 2061-15 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-15 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-15 provides excellent heat resistance, impact strength.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM Data |
Styron CALIBRE™ 300EP 22 Polycarbonate, General Purpose CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent p.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM Data |
Styron CALIBRE™ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 200-23 Polycarbonate Resin Overview: CALIBREâ„¢ 200-23 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 302EP-22 Polycarbonate Resin Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi.. |
|||
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | ASTM D1822, Type S |
Styron CALIBREâ„¢ 303 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |