Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00250 GPa | 0.363 ksi | ASTM D412 |
Multibase Multi-Flex® TPE A 7101 BLK Ash is 36.2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ISO/R527 |
Polykemi AB POLYelast TPE E606 Thermoplastic Elastomer, EPDM-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z650A Thermoplastic Elastomer, SEBS-based, Co-injection Grade Information provided by Polykemi AB |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ISO 37 |
Huntsman AVALON® 65 AB Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ISO 37 |
Huntsman AVALON® 65 AK-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ISO 37 |
Huntsman AVALON® 65 AC Thermoplastic Polyurethane Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ISO 37 |
Huntsman AVALON® 65 AE Thermoplastic Polyurethane Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ISO 37 |
Huntsman AVALON® 65 AK Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ASTM D412 |
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 Molded Brake Cup FormulationNordel® IP 4640 |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | 20 in/min; ASTM D412 (Dumbbells) |
DuPont Performance Polymers Kalrez® 8575 FFKM Perfluoroelastomer Kalrez® Sahara™ 8575 is specially formulated for improved performance in etching, ashing and stripping processes, offers lower cost of ownership with reduced contamination and longer seal life. Th.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR7060 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6153 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ASTM D 638 |
API Megol AM DP2268/65PA12 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | ISO 37 |
AlphaGary Evoprene™ Super G 949 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |