Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

API Megol AM DP2268/65PA12 SEBS Adhesion Modified Overmolding for PA

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer A.P.I. SpA
Trade Name Megol AM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF API Megol AM DP2268/65PA12 SEBS Adhesion Modified Overmolding for PA.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as there are no VOC emissions from adhesives and, as the components are not made from a range of incompatible materials, they are more easily recycled at the end of their useful life. The over-molding process can be used in highly technical applications such as components for the automotive industry, shells and casings for power tools, parts for domestic appliances, and seals which can be molded directly onto the frame.Information provided by A.P.I. SpA
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 65

@Time 15.0 sec
65

@Time 0.00417 hour
ASTM D 2240
Tensile Strength 9.50 MPa
1380 psi
ASTM D 638
Elongation at Break 700 %
700 %
ASTM D 638
100% Modulus 0.00250 GPa
0.363 ksi
ASTM D 638
300% Modulus 0.00440 GPa
0.638 ksi
ASTM D 638
Tear Strength 44.0 kN/m
251 pli
ASTM D 624
Compression Set 46 %

@Temperature 23.0 °C,
Time 259000 sec
46 %

@Temperature 73.4 °F,
Time 72.0 hour
ASTM D 395
78 %

@Temperature 70.0 °C,
Time 86400 sec
78 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D 395
92 %

@Temperature 100 °C,
Time 86400 sec
92 %

@Temperature 212 °F,
Time 24.0 hour
ASTM D 395
Descriptive Properties Value Comments
Compatibility PA12
Food contact On Request
Hygroscopicity Slightly
Main Features Easy Processability
Ozone Aging Resistance Excellent
72h, 40°C, 200 ppcm, Tension = 20%
Processing Injection Molding
Weathering Good
Users viewing this material also viewed the following: