Material Notes:
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and translucencyOil resistanceFast cycle timesOutstanding abrasion and scratch resistancePerfect color match with masterbatchesRubber-like look and feelExcellent bonding.Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 37
Elongation at Break 700 %
700 %
ISO 37
100% Modulus 0.00250 GPa
0.363 ksi
ISO 37
300% Modulus 0.00500 GPa
0.725 ksi
ISO 37
Tear Strength 40.0 kN/m
228 pli
ISO 34B
Abrasion 60
60
mm<sup>3</sup>; ISO 4649
Descriptive Properties Value Comments
Ross Flex -10°C, BS 5131