Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
Network Polymers Softflex® 2701T Transparent Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
Network Polymers Softflex® 2910 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Hi-Sil 233 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | 0.025" extruded film; DIN 53504 |
Huntsman IROGRAN® PS455-200 TPU-Polyester Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-360A Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | |
Kuraray SEPTON® H5127 Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO 37 |
Kuraray SEPTON® S4030 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO 527 |
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane Pearlbond™ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 402601S SBS Based Material, 60A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 500550S SEBS Based Material, Unfilled Qualities, 55A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 500600S SEBS Based Material, Unfilled Qualities, 60A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502550S SEBS Based Material, Unfilled Qualities, 55A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502600S SEBS Based Material, Unfilled Qualities, 60A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 600600S SEBS Based Material, Filled Qualities, 60A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 602550S SEBS Based Material, Filled Qualities, 55A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 660550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 660600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 662550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 662600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO 37 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Extrusion, Natural, Halogen Free Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770R Highly Extended Low-Cost Hose FormulationNordel® IP 4770R |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 600550S SEBS Based Material, Filled Qualities, 55A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6150 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
100% Modulus | 0.00200 - 0.0120 GPa | 0.290 - 1.74 ksi | |
Dow Advanta® 3302 Specialty Elastomer
(discontinued **) Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000.. |
|||
100% Modulus | 0.00200 - 0.0120 GPa | 0.290 - 1.74 ksi | |
Dow Advanta® 3650 Specialty Elastomer
(discontinued **) Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000.. |