Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00140 GPa | 0.203 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z506 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | TPE-0153 (ASTM D 412) |
ExxonMobil Santoprene® 8211-45W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | ISO 37 |
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | 0.025" extruded film; DIN 53504 |
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN .. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | Unfilled Tyrin compound; ASTM D412 |
Dow Tyrin® 3615P Chlorinated Polyethylene Elastomer 36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | Unfilled Tyrin compound; ASTM D412 |
Dow Tyrin® 4211P Chlorinated Polyethylene Elastomer 42% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | Unfilled Tyrin compound; ASTM D412 |
Dow Tyrin® 3611P Chlorinated Polyethylene Elastomer 36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | Unfilled Tyrin compound; ASTM D412 |
Dow Tyrin® 3623A Chlorinated Polyethylene Elastomer 36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | Unfilled Tyrin compound; ASTM D412 |
Dow Tyrin® CM2136P Chlorinated Polyethylene Elastomer 36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |
|||
100% Modulus | 0.00140 - 0.00400 GPa | 0.203 - 0.580 ksi | ASTM D 638 |
API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | ISO 37 |
AlphaGary Evoprene™ 3275 Standard SBS Thermoplastic Elastomer Compound |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | ISO 37 |
AlphaGary Evoprene™ Super G 948 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z557 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5616 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 4085 Chlorosulfonated Polyethylene Rubber, Gum Compound
(discontinued ** Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Reinforcing fillers not needed.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5697 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
100% Modulus | 0.00140 GPa | 0.203 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Gum Compound
(discontinued **)& Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Reinforcing fillers not needed.. |