Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Fumed Silica - Wacker HK N20

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Fumed Silica - Wacker HK N20.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100.0Zinc Stearate0.5MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur1.5Cumar P1010.0Fumed Silica - Wacker HK N2020All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 60
>= 60
Tensile Strength, Yield 32.0 MPa
4640 psi
Elongation at Yield 623 %
623 %
100% Modulus 0.00140 GPa
0.203 ksi
200% Modulus 0.00210 GPa
0.305 ksi
300% Modulus 0.00330 GPa
0.479 ksi
Tear Strength 36.8 kN/m
210 pli
Die C
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 68.3 °C
0.167 hour

@Temperature 155 °F
Press cured
Descriptive Properties Value Comments
DIN Abrasion (mm³) 30.8
Users viewing this material also viewed the following: