Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00700 GPa | 1.02 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | DIN 53504 |
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ISO 37 |
Huntsman AVALON® 90 AE Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ISO 37 |
Huntsman AVALON® 90 AHT DP Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | Press-cured 5 minutes at 190°C |
DuPont Vamac® DP DIAK No. 7 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1490IV Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D412 |
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ISO 37 |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D412 |
Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane Features: Matte finish, superior durabilityUses: Extrusion – wire and cable, General applicationAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | Cured 10 minutes at 180°C |
DuPont Vamac® DP 5.5 phr Peroxide Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1685AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | DIN 53504 |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer unmatched toughness and d.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D638 |
ELASTO UK Dryflex® 420351S SBS Based Material, 35D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D638 |
ELASTO UK Dryflex® 422351S SBS Based Material, 35D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1690AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00700 GPa | 1.02 ksi | DIN 53504 |
Lubrizol ESTANE® T5191 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |