Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00172 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00172 GPa
0.249 ksi
ASTM D412
Network Polymers Softflex® 0921
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
ASTM D412
Huntsman KRYSTALFLEX® PE 499 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
100% Modulus 0.00172 GPa
0.249 ksi
Shin-Etsu Silicones LIMSâ„¢ KEG2002-50A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
100% Modulus 0.00172 GPa
0.249 ksi
Shin-Etsu Silicones LIMSâ„¢ KEG2000-50A/B Elastomer
KEG2000-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Atomite Whiting Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus >= 0.00172 GPa
>= 0.250 ksi
Compound Property
Arlon 10502N060 0.060" (1.52 mm) Cured/Post-Cured Unsupported Silicone Rubber
Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t..
100% Modulus >= 0.00172 GPa
>= 0.250 ksi
Compound Property
Arlon 10502R010 0.010" (.254 mm) Cured/Post-Cured Unsupported Silicone Rubber
Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to..
100% Modulus >= 0.00172 GPa
>= 0.250 ksi
Compound Property
Arlon 10502R030 0.040" (1.02 mm) Cured/Post-Cured Unsupported Silicone Rubber
Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t..
100% Modulus >= 0.00172 GPa
>= 0.250 ksi
Tension, Silicone Property
Arlon 41400R030 0.030" Uncured, Unsupported Silicone Rubber on a Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
100% Modulus 0.00172 GPa
0.249 ksi
Average
Arlon Thermavac® 0.030" (0.762 mm) Uncured Silicone Vacuum Bagging (30400N030)
Uncured, unsupported silicone rubber with a thickness of 0.030 in ± 0.003 (0.76 mm ± 0.038) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.003 in. (0.8 mm) polyethylene interleave...
100% Modulus 0.00172 GPa
0.249 ksi
Average
Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502N060)
Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15 ); 0.003 in. (0.8 mm) polyethylene interleave. Color: Translucent. Weight: 2339 g/m² ± 234 (69.0..
100% Modulus 0.00172 GPa
0.249 ksi
Average
Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502R060)
Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15); 0.003 in. (0.8 mm) polyethylene interleave. The shelf life is defined as the duration of time for..
100% Modulus 0.00172 GPa
0.250 ksi
ASTM D638
Colorite Polymers 4875 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Atomite Whiting Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00172 GPa
0.250 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Copyright © lookpolymers.com All Rights Reserved