Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Sulfur Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Sulfur Cure.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5Cumar P1010.0Hi-Sil 23350.0AC Poly 617A2.0MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur1.5All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength, Yield 20.15 MPa
2922 psi
Elongation at Yield 671 %
671 %
100% Modulus 0.00172 GPa
0.250 ksi
200% Modulus 0.00301 GPa
0.436 ksi
300% Modulus 0.00509 GPa
0.738 ksi
Tear Strength 51.5 kN/m
294 pli
Die C
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 155 °C
0.250 hour

@Temperature 311 °F