Polymer Property : Impact Test = 160 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 217 J

@Thickness 0.250 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.00984 in,
Temperature -40.0 °F
Rotomolded samples; ARM Method
NOVA Chemicals Novapol® TR-0535-UI Hexene MDPE Rotational Molding Resin
TR-0530-UI complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UI is su..
Impact Test 217 J

@Thickness 0.250 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.00984 in,
Temperature -40.0 °F
Rotomolded samples; ARM Method
NOVA Chemicals Novapol® TR-0535-UIG Hexene MDPE Rotational Molding Resin
TR-0530-UIG complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UIG is ..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
rotomolded; ARM Method
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin  (discontinued **)
Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8360.29 Rotational Molding Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LL 8360.29 Linear Low Density Polyethylene Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LLP 8360.29 Linear Low Density Polyethylene Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLP8360.29 Rotational Molding Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLP8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLP8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8360 Rotational Molding Resin  (discontinued **)
LL 8360 is a linear low density hexene copolymer designed to provide good processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications tha..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8555.67 Rotational Molding Resin  (discontinued **)
LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir..
Impact Test 217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
rotomolded; ARM Method
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin  (discontinued **)
Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera..