Mechanical Properties Metric English Comments
Impact Test 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® C1950 PC+ABS
Low viscosity injection molding resin.This data was supplied by SABIC-IP for the Americas region.
Impact Test 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS
Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Americas region.
Impact Test 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific)
Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Geloy XTWM200 ASA
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region.
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact; Total Energy; ASTM-D3763
Ineos ABS Lustran® 288 ABS, Injection Molding Grade
Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Multiaxial Impact; E-fail; 0.100 in. thickness, 1.57 in. ring, 0.5 in. dart, 3.46 m/s velocity
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade
Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g..
Impact Test 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Total Penetration Energy; ISO 6603-2
Borealis Bormod™ BE961MO Polypropylene for Injection Molding
Bormod BE961MO is an heterophasic copolymer characterized by an optimum combination of high stiffness, low creep and very high impact strength.Bormod BE961MO is a new generation grade for very fast ..
Impact Test 40.0 J

@Temperature 0.000 °C
29.5 ft-lb

@Temperature 32.0 °F
ASTM D3763
Diamond Polymers Centrex® 810 Injection Molding Grade
Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and ..
Impact Test 40.0 J

@Thickness 4.00 mm
29.5 ft-lb

@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Assab Steels ASP 23 Cold Work Steel
ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope..