Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 152 MPa | 22000 psi | Ultimate; TM R050-38 |
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
PolyOne Edgetek® PS-30GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Compressive Strength | 152 MPa | 22000 psi | |
Poco Graphite EDM-AF5 EDM Graphite POCO's EDM-AF5 is the only graphite electrode material available on the market today with an average particle size of less than one micron. This particle structure gives EDM-AF5 superior strength, p.. |
|||
Compressive Strength | 152 MPa | 22000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet) |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
IDI Composites 44-1 Thermoset Polyester, Molding Multi-purpose medium strength material with excellent moldability and low cost.Data provided by the manufacturer. |
|||
Compressive Strength | 152 MPa | 22000 psi | |
Haysite H254 Polyester Laminate Solder Pallet and Work Holder Sheet A Static dissipative sheet material for use in electronic assembly. Resistant to hot solder and solvents. Standard color is blue/grey. Available thicknesses from.. |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG-F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Sumitomo Bakelite North America RX® 3-1-501N-P Mineral Filled Diallyl Phthalate Mineral filled, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG-F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Compressive Strength | 152 MPa | 22000 psi | ASTM D695 |
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK) TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels.. |
|||
Compressive Strength | <= 152 MPa | <= 22000 psi | ASTM D695 |
Ensinger Tecatron® XP-81 Compression Molded PPS Compound, Filled with 15% Graphite and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 1902 Mineral Filled Alkyd BMC 1902 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression molding. It was developed primarily for applications requiring very good impact and flex.. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose materia.. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Compressive Strength | 152 - 193 MPa | 22000 - 28000 psi | |
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl.. |
|||
Compressive Strength | 152 - 193 MPa | 22000 - 28000 psi | |
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab.. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e.. |
|||
Compressive Strength | 152 - 179 MPa | 22000 - 26000 psi | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Compressive Strength | 152 - 165 MPa | 22000 - 24000 psi | |
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re.. |
|||
Compressive Strength | 152 MPa | 22000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet) |
|||
Compressive Strength | 152 MPa | 22000 psi | Ultimate; TM R050-38 |
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |