Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 88.0 MPa | 12800 psi | 10% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 510 Polyethylene Terephthalate Application: friction bearings, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing |
Sharadaa Ceramics PCF (SIC) Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing |
Sharadaa Ceramics PCF60-2 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing |
Sharadaa Ceramics PCF70 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing |
Sharadaa Ceramics PCF80 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing |
Sharadaa Ceramics PCF90 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing |
Sharadaa Ceramics HA 88X High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 88.0 MPa | 12800 psi | ASTM D695 |
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information .. |
|||
Compressive Strength | 88.0 MPa | 12800 psi | ASTM D695 |
Sumitomo Bakelite North America SI 9550 Silicone Compound SI 9550 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated tempera.. |
|||
Compressive Strength | 88.3 MPa | 12800 psi | ASTM D695 |
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It .. |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories COD-2 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 88.3 MPa | <= 12800 psi | Cold Crushing Strength |
Chosun Refractories CUN-B937 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories SAL85N Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories SAL90 Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories SAL90CR Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories SAL95S Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories SAL99 Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories SAL99C Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories SB65S Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories SC80 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa | 12800 psi | Cold Crushing Strength |
Chosun Refractories AH-1 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.0 MPa | 12800 psi | ASTM D695 |
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp.. |