Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories SAL95S Special High Alumina brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chosun Refractories SAL95S Special High Alumina brick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.15 g/cc
0.114 lb/in³
Porosity 18 %
18 %
Mechanical Properties Metric English Comments
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 7.40 µm/m-°C

@Temperature 1000 °C
4.11 µin/in-°F

@Temperature 1830 °F
Shrinkage 0.00 %

@Temperature 1500 °C,
Time 7200 sec
0.00 %

@Temperature 2730 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 96 %
96 %
Fe2O3 0.20 %
0.20 %
Descriptive Properties Value Comments
Main Application Ammonia plant Carbon productor Rotary kiln Shaft kiln Various High-temp.
Refractories Under Load(2kg/?,T2?) 1,700 T2
Refractoriness (SK) 41
Users viewing this material also viewed the following: