Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 80.0 MPa | 11600 psi | Cold Crushing Strength |
Gouda Vuurvast AC 85-5 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. A good volume stability at very high temperatures. Application: chemical incinerators, combustion chambers for very high temperatur.. |
|||
Compressive Strength | 80.0 MPa | 11600 psi | Cold Crushing Strength |
Gouda Vuurvast AC 90-8 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. The 8% chromium-oxide addition gives good volume stability at very high temperatures. Applications: chemical incinerators, combusti.. |
|||
Compressive Strength | 80.0 MPa | 11600 psi | Cold Crushing Strength |
Gouda Vuurvast AK 85 K Dense Refractory Brick Description: Corundum based bricks with a mullite bond. Application: rotating incinerator furnacesRemarks: This data represents average values, obtained from samples that were cut from standard bric.. |
|||
Compressive Strength | 80.0 MPa | 11600 psi | Cold Crushing Strength |
Gouda Vuurvast LP 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. The extremely low porosity results in a very good slag resistance, a good abrasion resistance and high.. |
|||
Compressive Strength | 80.0 MPa | 11600 psi | Cold Crushing Strength |
Gouda Vuurvast AK 85 KP Dense Refractory Brick Description: This corundum based phosphate bond brick is characterized by a very low porosity, high slag resistance and high strength. Application: rotating incinerator furnaces.Remarks: This data r.. |
|||
Compressive Strength | 80.0 MPa | 11600 psi | ASTM D695 |
ScanTube PVDF Tubing Information provided by ScanTube, Inc. |
|||
Compressive Strength | 80.0 MPa | 11600 psi | ASTM D695 |
Unitika U-8400H U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |
|||
Compressive Strength | 80.0 MPa @Strain 3.50 % |
11600 psi @Strain 3.50 % |
DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Compressive Strength | 80.0 MPa | 11600 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | >= 80.0 MPa | >= 11600 psi | Axial; IEC 1212-2 4.2 |
Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube Used in mechanical and electrical applications. High mechanical strength. Good arc and tracking resistance. Information provided by Hippe. |
|||
Compressive Strength | >= 80.0 MPa | >= 11600 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 42 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Compressive Strength | >= 80.0 MPa | >= 11600 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 43 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Very coarse weave (less than 18 threads per cm).Information provided by Hippe. |
|||
Compressive Strength | >= 80.0 MPa | >= 11600 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CP 21 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal relative humidity.Information provided by Hippe. |
|||
Compressive Strength | >= 80.0 MPa | >= 11600 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CP 42 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity. Lower mechanical and electrical properties than PF CP 41.Information.. |
|||
Compressive Strength | >= 80.0 MPa | >= 11600 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe PF WV 303 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical applications. Good mechanical properties.Information provided by Hippe. |
|||
Compressive Strength | >= 80.0 MPa | >= 11600 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical and electrical applications.Information provided by Hippe. |
|||
Compressive Strength | 80.0 MPa @Temperature 22.8 °C |
11600 psi @Temperature 73.0 °F |
ASTM D695 |
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent.. |
|||
Compressive Strength | >= 80.0 MPa | >= 11600 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CP 22 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube High-voltage, electrical applications at power frequencies. High electric strength in oil.Information provided by Hippe. |
|||
Compressive Strength | 80.0 - 120 MPa | 11600 - 17400 psi | |
Alliance BCN-11 Bonded (Composite) Magnetic Material |
|||
Compressive Strength | 80.0 - 120 MPa | 11600 - 17400 psi | |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
Compressive Strength | 80.0 MPa | 11600 psi | ASTM D695 |
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade) 3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate.. |
|||
Compressive Strength | 80.0 - 120 MPa | 11600 - 17400 psi | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Compressive Strength | 80.0 - 120 MPa | 11600 - 17400 psi | |
Alliance BCN-12 Bonded (Composite) Magnetic Material |
|||
Compressive Strength | 80.0 - 120 MPa | 11600 - 17400 psi | |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
Compressive Strength | 80.0 - 120 MPa | 11600 - 17400 psi | |
Alliance BCN-15 Bonded (Composite) Magnetic Material |
|||
Compressive Strength | 80.0 - 120 MPa | 11600 - 17400 psi | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |
|||
Compressive Strength | >= 80.0 MPa | >= 11600 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CP 43 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical applications and low-voltage electrical applications.Information provided by Hippe. |