Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 124 MPa | 18000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet) |
|||
Compressive Strength | 124 MPa | 18000 psi | Break; TM R050-38 |
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11.. |
|||
Compressive Strength | 124 MPa | 18000 psi | Ultimate; TM R050-38 |
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Compressive Strength | 124 MPa | 18000 psi | |
Poco Graphite AXM-5Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | ASTM D695 |
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Compressive Strength | 124 - 138 MPa | 18000 - 20000 psi | ASTM D695 |
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Compressive Strength | 124 MPa @Thickness 12.7 mm |
18000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP615 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated .. |
|||
Compressive Strength | 124 MPa | 18000 psi | |
Haysite 42100 Polyester SMC, 22% Glass Reinforced Haysite Grade 42100 is a fiber glass reinforced thermoset polyester sheet molding compound exhibiting excellent moldability. It is designed for compression molded parts requiring high strength and g.. |
|||
Compressive Strength | 124 MPa | 18000 psi | |
Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced The 44500 series sheet molding compound offers high strength and excellent resistance to corrosive agents. This compression molding grade is formulated with a vinyl ester resin system. |
|||
Compressive Strength | 124 MPa | 18000 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Compressive Strength | 124 MPa | 18000 psi | ASTM D695 |
Techmer ES Electrafil® J-1/CF/10 Nylon 66, 10% Carbon Fiber Reinforced |
|||
Compressive Strength | 124 MPa | 18000 psi | ASTM D695 |
Techmer ES Plaslube® J-4/30/TF/13/SI/2 NAT PA6/12 |
|||
Compressive Strength | >= 124 MPa | >= 18000 psi | |
Master Bond EP45HTAO Heat Resistant Epoxy for Structural Bonding Description: Master Bond Polymer Compound EP45HTAO is a two component thermally conductive epoxy compound for high performance structural bonding, and casting. It is suitable for applications where .. |
|||
Compressive Strength | 124 MPa | 18000 psi | ASTM D695 |
Westlake Plastics Zelux® 30% GF Polycarbonate 30% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Compressive Strength | >= 124 MPa | >= 18000 psi | |
Master Bond EP30QF Quartz Filled, Two Component Epoxy System Master Bond Polymer System EP30QF is a quartz filled, two component epoxy for high performance bonding, sealing, coating and casting that is formulated to cure at room temperature or more rapidly at.. |
|||
Compressive Strength | 124 MPa | 18000 psi | |
3M HGS18000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Compressive Strength | 124 MPa | 18000 psi | |
3M S60HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Compressive Strength | 124 - 138 MPa | 18000 - 20000 psi | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Compressive Strength | 124 - 145 MPa | 18000 - 21000 psi | |
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c.. |
|||
Compressive Strength | 124 - 138 MPa | 18000 - 20000 psi | |
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,.. |
|||
Compressive Strength | 124 - 138 MPa | 18000 - 20000 psi | |
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r.. |
|||
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | |
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding.. |
|||
Compressive Strength | 124 - 138 MPa | 18000 - 20000 psi | |
Bulk Molding Compounds BMC 1050 Thermoset Polyester BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e.. |
|||
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Compressive Strength | 124 - 159 MPa | 18000 - 23000 psi | |
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings. |
|||
Compressive Strength | 124 - 138 MPa | 18000 - 20000 psi | |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Compressive Strength | 124 - 138 MPa | 18000 - 20000 psi | |
Bulk Molding Compounds BMC 945 Conductive Grade Bulk Molding Compound BMC 945 is an ESD level Conductive grade of Bulk Molding Compound and is suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reacti.. |
|||
Compressive Strength | 124 MPa | 18000 psi | Ultimate; TM R050-38 |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |