Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 100 - 145 MPa | 14500 - 21000 psi | Type B, 5mm/min; ISO 604:2002 |
Nylacast Moly Cast Nylon 6, MoS2 Filled Nylacast Moly is part of the Cast Nylon 6 family. Its improved crystallization occurs by the addition of Molybdenum Disulphide. It includes MoS2, which is an extremely effective self dry lubricant w.. |
|||
Compressive Strength | 100 - 150 MPa | 14500 - 21800 psi | Injection; ISO 604 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Compressive Strength | 100 - 150 MPa | 14500 - 21800 psi | ISO 604 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Sample Type B, 5 mm/min; ISO 604:2002 |
Global EPP PET PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Sample Type B, 5 mm/min; ISO 604:2002 |
Global EPP PET SL PET + Solid Lubricant PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast AK 94 M Dense Refractory Brick Description: This mullite bonded, corundum brick combines a very good thermal shock resistance with a low creep as well as with resistance against a large variety of slags. (after 50 hours at 1650Â.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast AK 99 S Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast LP 60 AAP Dense Refractory Brick Description: Special low porosity quality for use under severe corrosive conditions, (for instance liquid slags). Moreover, this brick has been extra protected against slag attack because it also co.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast AK 85 PW Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. Application: aluminum holding furnaces.Remarks: This data represents average.. |
|||
Compressive Strength | 100 MPa | 14500 psi | |
SGL Carbon Group EK 40 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 100 - 120 MPa | 14500 - 17400 psi | ISO 604 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 22 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Coarse weave (18-30 threads per cm).Information provided by Hippe. |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 23 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Very coarse weave ( |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 32 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Compressive Strength | >= 100 MPa | >= 14500 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CC 34 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe. |
|||
Compressive Strength | 100 MPa | 14500 psi | EN ISO 604 |
Brandenburger S 2000 A Side Insulation S 2000 A is reinforced with load-bearing glass fibre mat with thermoset weave. A laminated aluminum lining provides additional heat-reflecting protection.Information provided by Brandenburger Isolie.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast LP 60 M Dense Refractory Brick Description: LP 60 M is a special low porosity, high strength material based on raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a ma.. |
|||
Compressive Strength | 100 MPa | 14500 psi | Cold Crushing Strength |
Gouda Vuurvast LP 97-3 Dense Refractory Brick Description: A high alumina quality brick containing a limited percentage of chromium oxide for improved slag resistance. The product has a very low silica- and iron oxide percentage so that it can .. |