Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 62.0 MPa | 8990 psi | at Break (NYP); ISO 527-1/-2 |
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data) Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l.. |
|||
Tensile Strength | 62.0 MPa | 8990 psi | ASTM D638 |
Kolon KOCETAL® K300EW Standard Grade Acetal Resin General injection molding grade, toughness is slightly improved. Applications: General injection molding products.Information provided by API-Kolon. |
|||
Tensile Strength | 62.0 MPa | 8990 psi | ASTM D638 |
Kolon KOCETAL® LF701 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Tensile Strength | 62.0 MPa | 8990 psi | ASTM D638 |
Kolon KOCETAL® TC702 Mineral Reinforced Acetal Resin Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Tensile Strength | 62.0 - 69.0 MPa | 8990 - 10000 psi | specimen type 1, 5 mm/mn; ASTM D638 |
Lucite International XL Sanitary Ware Acrylic Sheet Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an.. |
|||
Tensile Strength | 62.0 MPa @Strain 14.0 %, Temperature 40.0 °C |
8990 psi @Strain 14.0 %, Temperature 104 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 62.0 MPa @Temperature 23.0 °C |
8990 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612
(Unverified Data**) Zytel® FE3734 NC010 is an unreinforced, lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 62.0 MPa | 8990 psi | ISO 527-1 |
Sax Polymers SAXATEC 4115 Acrylonitrile Styrene Acrylate SAXATEC 4115 is a medium viscosity, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX .. |
|||
Tensile Strength | 62.0 MPa | 8990 psi | ISO 527-1 |
Sax Polymers SAXATEC 4120 Acrylonitrile Styrene Acrylate SAXATEC 4120 is a easy lowing, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym.. |