Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 186 MPa | 27000 psi | ASTM D-638 |
PlastiComp Complet® LCF40-PEI Polyetherimide, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long carbon fiber reinforcementInformation provided by PlastiC.. |
|||
Tensile Strength | 186 MPa | 27000 psi | ASTM D638 |
Kolon KOPA® KN333G30BL G/F Reinforced Nylon 66 G/F 30% reinforcedApplications Engine coversInformation provided by API-Kolon. |
|||
Tensile Strength | 186 MPa | 27000 psi | ASTM D638 |
Kolon KOPA® KN333G30CRN G/F Reinforced Nylon 66 Oil resistantApplications Surge tanksInformation provided by API-Kolon. |
|||
Tensile Strength | 186 MPa | 27000 psi | ASTM D638 |
Kolon KOPA® KN333G35CR G/F Reinforced Nylon 66 High thermal resistant, Weather resistant, dimensionally stableApplications Cylinder head coversInformation provided by API-Kolon. |
|||
Tensile Strength | 186 MPa | 27000 psi | ASTM D638 |
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66 EG-resistant, high strength, dimensionally stableApplications Coolant temperature control partsInformation provided by API-Kolon. |
|||
Tensile Strength | 186 MPa | 27000 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s.. |
|||
Tensile Strength | 186 MPa | 27000 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
Tensile Strength | 186 MPa | 27000 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 186 MPa | 27000 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 186 MPa | 27000 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Tensile Strength | 186 MPa | 27000 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hMR61LC1 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |