Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 13.0 MPa | 1890 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Tensile Strength | >= 13.0 MPa | >= 1890 psi | DIN 53504 |
NEXA® PFX8045 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
Tensile Strength | 13.0 MPa | 1890 psi | ASTM D2095 |
Permabond UV640 UV-curable Adhesive PERMABOND UV640 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Tensile Strength | 13.0 MPa @Strain 100 % |
1890 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B5DW2 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 13.0 - 18.0 MPa | 1890 - 2610 psi | ASTM D4894 |
Isoflon PTFE + 25% Carbon Polytetrafluoroethylene with 25% Carbon Properties:Improved compression and wear resistanceGood thermal conductivityLow permeabilityImproved coefficient of thermal expansion when combined with ceramicApplications: Seals recommended for h.. |
|||
Tensile Strength | 13.0 - 18.0 MPa | 1890 - 2610 psi | ASTM D4894 |
Isoflon PTFE + 25% Glass Polytetrafluoroethylene with 25% Glass Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityApplications: Dynamic seals with rotating or alternating motion.Information provided by Iso.. |
|||
Tensile Strength | >= 13.0 MPa | >= 1890 psi | extruded; ASTM D4894, ASTM D4745 |
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
Tensile Strength | 13.0 - 18.0 MPa | 1890 - 2610 psi | ASTM D4894 |
Isoflon PTFE +28% GL Blue-E glass-1% Blue Polytetrafluoroethylene with 28% GL-Blue-E glass-1% Blue (equivalent VX1) Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityInformation provided by Isoflon. |
|||
Tensile Strength | 13.0 MPa | 1890 psi | Crosslinked specimen; ISO 527 |
Fainplast Compounds Hax™ HFX 515 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com.. |
|||
Tensile Strength | 13.0 MPa @Strain 20.0 % |
1890 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 13.0 MPa @Strain 20.0 % |
1890 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan B 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 13.0 MPa @Strain 300 % |
1890 psi @Strain 300 % |
ISO 37 |
BASF Elastollan C 88 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 13.0 MPa @Strain 300 % |
1890 psi @Strain 300 % |
ISO 37 |
BASF Elastollan 1185 A FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 13.0 MPa @Strain 300 % |
1890 psi @Strain 300 % |
ISO 37 |
BASF Elastollan 1185 A WM TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 13.0 MPa @Strain 300 % |
1890 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 13.0 MPa | 1890 psi | |
AlphaGary Megolon™ IN700 Low Smoke Halogen Free Thermoplastic, fire retardant INSULATION compound designed to meet the requirements of the Spanish Cable Standard UNE 211002:2004 for Building Wire Cable 450/750V. This material has been formulated .. |
|||
Tensile Strength | 13.0 MPa | 1890 psi | ISO 527 |
Fainplast Compounds Hax™ HF 045/11 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, low shrinkageInformation provided by Fainplast Compounds |
|||
Tensile Strength | 13.0 MPa | 1890 psi | Plasticizer conc. in vinyl film 70 phr; ASTM D638 |
BASF Palatinol® N Diisononyl Phthalate Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl.. |
|||
Tensile Strength | >= 13.0 MPa | >= 1890 psi | extruded; ASTM D1708 |
Guarniflon PTFE G200 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Tensile Strength | >= 13.0 MPa | >= 1890 psi | molded; ASTM D1708 |
Guarniflon PTFE G200 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Tensile Strength | >= 13.0 MPa | >= 1890 psi | extruded; ASTM D4894, ASTM D4745 |
Guarniflon PTFE G458 Polytetrafluoroethylene 60% Bronze, 2% Carbon PTFE G Standard Compound with bronzeProperties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard .. |