Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D-638 |
Plaskolite Optix® CA - 87 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D-638 |
Plaskolite West Optix® CA - 87 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet) |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet) |
|||
Tensile Strength | 76.0 MPa | 11000 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Tensile Strength | 75.8 MPa @Temperature 22.8 °C |
11000 psi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet) |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Quantum PPSU Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)
(Unverified Data**) Udel P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aest.. |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Solvay Specialty Polymers Udel® M-2300 MR Polysulfone (PSU), Mold Release
(discontinued **) Udel M-2300 MR is an injection-moldable, low-color grade of polysulfone that is nearly water white in color. This material contains a mold release which aids part ejection when parts with low draft .. |
|||
Tensile Strength | 76.0 MPa @Temperature 23.0 °C |
11000 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 76.0 MPa | 11000 psi | ISO 527 |
Lucite International Diakon® CLG960 Acrylic Polymer Information provided by Lucite International |
|||
Tensile Strength | 75.9 MPa | 11000 psi | |
Henkel Hysol EA 9150 Composite Resin Low viscosity, toughened system formulated for resin transfer molding. 250°F / 121°C cure and service temperature.Application: Composite Binding |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7400 Polyphenylsulfone (PPSU) Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame.. |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU) Udel® P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved .. |
|||
Tensile Strength | >= 75.8 MPa @Temperature 23.9 °C |
>= 11000 psi @Temperature 75.0 °F |
|
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun.. |
|||
Tensile Strength | >= 75.8 MPa @Temperature 23.9 °C |
>= 11000 psi @Temperature 75.0 °F |
|
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy Master Bond EP112FLAO-1 is a toughened two component, high performance epoxy resin system featuring very good temperature resistance, fine thermal conductivity and electrical insulation values with .. |
|||
Tensile Strength | 75.5 MPa | 11000 psi | ASTM D638 |
E-Polymers TEKAMID® TB120CR Fast Crystallinity PA6 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
CIP Composites 100 Series Laminated Polymer Bearing Material The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated.. |
|||
Tensile Strength | 76.0 MPa @Strain 15.0 %, Temperature 0.000 °C |
11000 psi @Strain 15.0 %, Temperature 32.0 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Aaron Industries AAROPRENE® GFABS 4020 Glass Filled Acrylonitrile-Butadiene Styrene AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7300 Polyphenylsulfone (PPSU) Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame r.. |