Polymer Property : Tensile Strength = 3.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 3.10 MPa

@Strain 300 %
450 psi

@Strain 300 %
ISO 527
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
Tensile Strength >= 3.10 MPa
>= 450 psi
ASTM D412
Parker Chomerics CHO-FORM® 5515 Robotically Dispensed Gasketing
Description: CHO-FORM® 5515 One-component, thermal cure silicone system, with Ni/Graphite filler. Minimum cure temperature is 100°C (212°F). A low-cost solution for EMI shielding, it is specially..
Tensile Strength 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B65B1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3855 Polyvinyl Chloride, Flexible (PVC, Flexible)
XV3855 is a flexible (57A durometer) vinyl compound formulated from FDA-santioned raw materials. XV3855 Clear 1869 has been tested to USP Class VI.NOTE: All ingredients used in the formulation of th..
Tensile Strength 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible C6500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength >= 3.10 MPa
>= 450 psi
Compound Property
Arlon CP-338R Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Tensile Strength 3.10 MPa
450 psi
AlphaGary AlphaSeal™ 225 H Polyolefin Thermoplastic Elastomer
AlphaSeal™ 255 H is a polyolefin/TPE cap liner material used for milk bottle caps. AlphaSeal is formulated for low taste and low odor and exhibits good elastic recovery, abrasion resistance and low..
Tensile Strength 3.10 MPa
450 psi
average; perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..